MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Dyneon™ PFE 60 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provides a very broad chemical and thermal stability. Low viscosity provides good mold flow and is ideal for molding large parts. It is classified as FFKM per ASTM D1418.
    Features and Benefits:
  • Ideal for wet chemical, fluid handling, cleaning and chemical etching processes and for large parts for CPI and aerospace
  • Low metal ion content with low extractables in a wide range of chemicals
  • Upper use temperature of 220°C
  • Good compression set resistance
  • Good mold flow
  • Peroxide curable FFKM

Information provided by the Dyneon division of 3M.

Key Words: Formerly PFE 60Z
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.98 g/cc
Mooney Viscosity 60
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D2240
Tensile Strength at Break 17.9 MPaPress cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412
Elongation at Break 165 %Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412
100% Modulus 0.00110 GPa
@Strain 100 %
Press cure 10 Minutes @ 177°C, Post Cure 16 Hours @ 232°C; ASTM D412
Compression Set 49 %
@Treatment Temp. 200 °C,
Time 252000 sec
Method B, -214 O-rings, Aged 168 Hours, 25% Deformation; ASTM D395
 55 %
@Treatment Temp. 200 °C,
Time 605000 sec
Method B, -214 O-rings, Aged 168 Hours, 25% Deformation; ASTM D395
 56 %
@Treatment Temp. 230 °C,
Time 252000 sec
Method B, -214 O-rings, Aged 70 Hours, 25% Deformation; ASTM D395
 68 %
@Treatment Temp. 230 °C,
Time 605000 sec
Method B, -214 O-rings, Aged 168 Hours, 25% Deformation; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °C
Brittleness Temperature -35.0 °C
Transformation Temperature -2.00 °CTR10
 
Descriptive Properties
ColorOff White to translucent
FormSlab
MH, Maximum Toque13.4 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
ML, Minimum Torque2.0 inch-lb100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t2, Time to 2 Inch-lb Rise from Minimum0.6 Minute100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'50, Time to 50% Cure0.8 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289
t'90, Time to 90% Cure1.5 Minutes100 cpm, 0.5° Arc, 6 Minutes @ 177°C, ASTM D5289

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Dyneon™ 2299X Ultra High Viscosity Fluoroelastomer
3M Dyneon™ PFE 133TB High Temperature Perfluoroelastomer
3M Dyneon™ PFE 132TB High Temperature Perfluoroelastomer
3M Dyneon™ 81T High Temperature Perfluoroelastomer
3M Dyneon™ 301Z Translucent Perfluoroelastomer System

PDYL9973 / 129991

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.