Features PA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased flammability, glow wire 850°C. Application: Injection Moulding Information Provided by Plastcom spol. s r.o. |