MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Plastcom SLOVAMID 66 GF 30 FRA 3 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Features

PA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased flammability, glow wire 850°C.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.43 g/cc0.0517 lb/in³STN 64 0111
Linear Mold Shrinkage 0.0058 cm/cm0.0058 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0099 cm/cm0.0099 in/inSTN 64 0808
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiSTN EN ISO 527-2
Elongation at Break 2.0 %2.0 %STN EN ISO 527-2
Tensile Modulus 6.00 GPa870 ksiSTN EN ISO 527-2
Flexural Strength 180 MPa26100 psiSTN EN ISO 178
Flexural Modulus 5.50 GPa798 ksiSTN EN ISO 178
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -20.0 °C
26.2 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 6.00 J/cm²
@Temperature 23.0 °C
28.6 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched  1.20 J/cm²
@Temperature -20.0 °C
5.71 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmSTN IEC 60093
Surface Resistance 1.00e+13 ohm1.00e+13 ohmSTN IEC 60093
Dielectric Strength 40.0 kV/mm1020 kV/inSTN IEC 60243
Comparative Tracking Index 450 V450 VSTN 34 6468
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FSTN EN ISO 75/A
Vicat Softening Point 250 °C482 °FB; STN EN ISO 306
Flammability, UL94 V-2V-2
Glow Wire Test 850 °C1560 °FSTN IEC 60695-2-10
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 70.0 - 90.0 °C158 - 194 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPLACO056 / 106934

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.