MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Sandvik 2C48 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Sandvik 2C48 is a ferritic, heat resisting, stainless chromium steel, characterized by:
  • good resistance to reducing sulphurous gases
  • very good resistance to oxidation in air
  • good resistance to oil-ash corrosion
  • resistance to molten copper, lead and tin
  • This steel can be used at temperatures up to 1075 °C (1970 °F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel.

    Information provided by Sandvik

    ASTM 446-2; UNS S44600

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.60 g/cc0.275 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell B 9595
    Tensile Strength, Ultimate >= 450 MPa>= 65300 psi
    Tensile Strength, Yield >= 275 MPa
    @Strain 0.2 %
    >= 39900 psi
    @Strain 0.2 %
    Elongation at Break >= 20 %>= 20 %
    Modulus of Elasticity 195 GPa28300 ksi
     120 GPa
    @Temperature 1000 °C
    17400 ksi
    @Temperature 1830 °F
     125 GPa
    @Temperature 800 °C
    18100 ksi
    @Temperature 1470 °F
     145 GPa
    @Temperature 600 °C
    21000 ksi
    @Temperature 1110 °F
     180 GPa
    @Temperature 400 °C
    26100 ksi
    @Temperature 752 °F
     190 GPa
    @Temperature 200 °C
    27600 ksi
    @Temperature 392 °F
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear  10.0 µm/m-°C
    @Temperature 30.0 - 100 °C
    5.56 µin/in-°F
    @Temperature 86.0 - 212 °F
     10.0 µm/m-°C
    @Temperature 30.0 - 100 °C
    5.56 µin/in-°F
    @Temperature 86.0 - 212 °F
     10.0 µm/m-°C
    @Temperature 30.0 - 200 °C
    5.56 µin/in-°F
    @Temperature 86.0 - 392 °F
     10.5 µm/m-°C
    @Temperature 30.0 - 300 °C
    5.83 µin/in-°F
    @Temperature 86.0 - 572 °F
     11.0 µm/m-°C
    @Temperature 30.0 - 500 °C
    6.11 µin/in-°F
    @Temperature 86.0 - 932 °F
     11.0 µm/m-°C
    @Temperature 30.0 - 500 °C
    6.11 µin/in-°F
    @Temperature 86.0 - 932 °F
     11.5 µm/m-°C
    @Temperature 30.0 - 700 °C
    6.39 µin/in-°F
    @Temperature 86.0 - 1290 °F
     13.0 µm/m-°C
    @Temperature 30.0 - 900 °C
    7.22 µin/in-°F
    @Temperature 86.0 - 1650 °F
     13.5 µm/m-°C
    @Temperature 30.0 - 1000 °C
    7.50 µin/in-°F
    @Temperature 86.0 - 1830 °F
    Specific Heat Capacity  0.475 J/g-°C
    @Temperature 20.0 °C
    0.114 BTU/lb-°F
    @Temperature 68.0 °F
     0.520 J/g-°C
    @Temperature 100 °C
    0.124 BTU/lb-°F
    @Temperature 212 °F
     0.555 J/g-°C
    @Temperature 200 °C
    0.133 BTU/lb-°F
    @Temperature 392 °F
     0.595 J/g-°C
    @Temperature 300 °C
    0.142 BTU/lb-°F
    @Temperature 572 °F
     0.625 J/g-°C
    @Temperature 400 °C
    0.149 BTU/lb-°F
    @Temperature 752 °F
     0.680 J/g-°C
    @Temperature 900 °C
    0.163 BTU/lb-°F
    @Temperature 1650 °F
     0.695 J/g-°C
    @Temperature 800 °C
    0.166 BTU/lb-°F
    @Temperature 1470 °F
     0.710 J/g-°C
    @Temperature 500 °C
    0.170 BTU/lb-°F
    @Temperature 932 °F
     0.715 J/g-°C
    @Temperature 1000 °C
    0.171 BTU/lb-°F
    @Temperature 1830 °F
     0.720 J/g-°C
    @Temperature 700 °C
    0.172 BTU/lb-°F
    @Temperature 1290 °F
     0.760 J/g-°C
    @Temperature 1100 °C
    0.182 BTU/lb-°F
    @Temperature 2010 °F
     0.795 J/g-°C
    @Temperature 600 °C
    0.190 BTU/lb-°F
    @Temperature 1110 °F
    Thermal Conductivity  20.0 W/m-K
    @Temperature 20.0 °C
    139 BTU-in/hr-ft²-°F
    @Temperature 68.0 °F
     21.0 W/m-K
    @Temperature 100 °C
    146 BTU-in/hr-ft²-°F
    @Temperature 212 °F
     22.0 W/m-K
    @Temperature 200 °C
    153 BTU-in/hr-ft²-°F
    @Temperature 392 °F
     23.0 W/m-K
    @Temperature 400 °C
    160 BTU-in/hr-ft²-°F
    @Temperature 752 °F
     23.0 W/m-K
    @Temperature 300 °C
    160 BTU-in/hr-ft²-°F
    @Temperature 572 °F
     24.0 W/m-K
    @Temperature 500 °C
    167 BTU-in/hr-ft²-°F
    @Temperature 932 °F
     24.0 W/m-K
    @Temperature 700 °C
    167 BTU-in/hr-ft²-°F
    @Temperature 1290 °F
     25.0 W/m-K
    @Temperature 600 °C
    174 BTU-in/hr-ft²-°F
    @Temperature 1110 °F
     28.0 W/m-K
    @Temperature 900 °C
    194 BTU-in/hr-ft²-°F
    @Temperature 1650 °F
     34.0 W/m-K
    @Temperature 1100 °C
    236 BTU-in/hr-ft²-°F
    @Temperature 2010 °F
     34.0 W/m-K
    @Temperature 1000 °C
    236 BTU-in/hr-ft²-°F
    @Temperature 1830 °F
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.090 %0.090 %
    Chromium, Cr 23.5 %23.5 %
    Iron, Fe 74.9 %74.9 %As Balance
    Manganese, Mn 0.80 %0.80 %
    Nitrogen, N 0.20 %0.20 %
    Phosphorus, P <= 0.030 %<= 0.030 %
    Silicon, Si 0.50 %0.50 %
    Sulfur, S <= 0.015 %<= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Overview of materials for T 300 Series Stainless Steel
    AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

    NSANDV226 / 19120

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.