MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Sandvik 2C48 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Ferritic; Stainless Steel

Material Notes: Sandvik 2C48 is a ferritic, heat resisting, stainless chromium steel, characterized by:
  • good resistance to reducing sulphurous gases
  • very good resistance to oxidation in air
  • good resistance to oil-ash corrosion
  • resistance to molten copper, lead and tin
  • This steel can be used at temperatures up to 1075 °C (1970 °F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel.

    Information provided by Sandvik

    ASTM 446-2; UNS S44600

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 7.60 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell B 95
    Tensile Strength, Ultimate >= 450 MPa
    Tensile Strength, Yield >= 275 MPa
    @Strain 0.2 %
    Elongation at Break >= 20 %
    Modulus of Elasticity 195 GPa
     120 GPa
    @Temperature 1000 °C
     125 GPa
    @Temperature 800 °C
     145 GPa
    @Temperature 600 °C
     180 GPa
    @Temperature 400 °C
     190 GPa
    @Temperature 200 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 10.0 µm/m-°C
    @Temperature 30.0 - 100 °C
     10.0 µm/m-°C
    @Temperature 30.0 - 100 °C
     10.0 µm/m-°C
    @Temperature 30.0 - 200 °C
     10.5 µm/m-°C
    @Temperature 30.0 - 300 °C
     11.0 µm/m-°C
    @Temperature 30.0 - 500 °C
     11.0 µm/m-°C
    @Temperature 30.0 - 500 °C
     11.5 µm/m-°C
    @Temperature 30.0 - 700 °C
     13.0 µm/m-°C
    @Temperature 30.0 - 900 °C
     13.5 µm/m-°C
    @Temperature 30.0 - 1000 °C
    Specific Heat Capacity 0.475 J/g-°C
    @Temperature 20.0 °C
     0.520 J/g-°C
    @Temperature 100 °C
     0.555 J/g-°C
    @Temperature 200 °C
     0.595 J/g-°C
    @Temperature 300 °C
     0.625 J/g-°C
    @Temperature 400 °C
     0.680 J/g-°C
    @Temperature 900 °C
     0.695 J/g-°C
    @Temperature 800 °C
     0.710 J/g-°C
    @Temperature 500 °C
     0.715 J/g-°C
    @Temperature 1000 °C
     0.720 J/g-°C
    @Temperature 700 °C
     0.760 J/g-°C
    @Temperature 1100 °C
     0.795 J/g-°C
    @Temperature 600 °C
    Thermal Conductivity 20.0 W/m-K
    @Temperature 20.0 °C
     21.0 W/m-K
    @Temperature 100 °C
     22.0 W/m-K
    @Temperature 200 °C
     23.0 W/m-K
    @Temperature 400 °C
     23.0 W/m-K
    @Temperature 300 °C
     24.0 W/m-K
    @Temperature 500 °C
     24.0 W/m-K
    @Temperature 700 °C
     25.0 W/m-K
    @Temperature 600 °C
     28.0 W/m-K
    @Temperature 900 °C
     34.0 W/m-K
    @Temperature 1100 °C
     34.0 W/m-K
    @Temperature 1000 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C 0.090 %
    Chromium, Cr 23.5 %
    Iron, Fe 74.9 %As Balance
    Manganese, Mn 0.80 %
    Nitrogen, N 0.20 %
    Phosphorus, P <= 0.030 %
    Silicon, Si 0.50 %
    Sulfur, S <= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Overview of materials for T 300 Series Stainless Steel
    AISI 1045 Steel, cold drawn, 19-32 mm (0.75-1.25 in) round

    NSANDV226 / 19120

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.