MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccResin Density
 2.60 g/ccFiber Density
Filler Content 50.0 %Fiber Volume
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 415 MPa90º, RT, Dry; EN2561
 510 MPaRT; Dry; EN2561
 270 MPa
@Temperature 75.0 °C
Wet; EN2561
 270 MPa
@Temperature 100 °C
Wet; EN2561
 270 MPa
@Temperature 75.0 °C
90º, Wet; EN2561
 300 MPa
@Temperature 100 °C
90º, Wet; EN2561
Tensile Modulus 26.0 GPa90º, RT, Dry; EN2561
 29.0 GPaRT; Dry; EN2561
 25.0 GPa
@Temperature 100 °C
90º, Wet; EN2561
 26.0 GPa
@Temperature 75.0 °C
90º, Wet; EN2561
 27.0 GPa
@Temperature 100 °C
Wet; EN2561
 28.0 GPa
@Temperature 75.0 °C
Wet; EN2561
Compressive Yield Strength 460 MPa90º, RT, Dry; DIN65380
 500 MPaRT; Dry; DIN65380
 320 MPa
@Temperature 100 °C
90º, Wet; DIN65380
 360 MPa
@Temperature 100 °C
Wet; DIN65380
 380 MPa
@Temperature 75.0 °C
Wet; DIN65380
 400 MPa
@Temperature 75.0 °C
90º, Wet; DIN65380
Compressive Modulus 27.0 GPa90º, RT, Dry; DIN65380
 30.0 GPaRT; Dry; DIN65380
 25.0 GPa
@Temperature 100 °C
90º, Wet; DIN65380
 26.0 GPa
@Temperature 75.0 °C
Wet; DIN65380
 26.0 GPa
@Temperature 100 °C
Wet; DIN65380
 26.0 GPa
@Temperature 75.0 °C
90º, Wet; DIN65380
Shear Strength 80.0 MPaIn-Plane, RT, Dry; EN6031
 83.0 MPa0º, ILSS (Short Beam), RT, Dry; EN2563
 37.0 MPa
@Temperature 100 °C
0º, ILSS (Short Beam), Wet; EN2563
 43.0 MPa
@Temperature 75.0 °C
0º, ILSS (Short Beam), Wet; EN2563
 70.0 MPa
@Temperature 100 °C
In-Plane, Wet; EN6031
 75.0 MPa
@Temperature 75.0 °C
In-Plane, Wet; EN6031
 
Processing PropertiesOriginal ValueComments
Shelf Life 14.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Cured Thickness per Ply (cm)0.23

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Solvay CYCOM® 919 Epoxy Prepreg System with Woven E Glass Fiber 7781
Park Aerospace Nelcote® E-718 Epoxy Prepreg, 7781 E-Glass Reinforced
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Overview of materials for High Carbon Steel

PHEXC157 / 98627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.