Description: Topical MVTR and water resistance coating Usage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include roll wrap, produce boxes, poultry boxes and anywhere packaged goods require protection from water and or moisture vapor. Application Data: VaporCoat® 330C is best applied by rod coater in-line or off-line at the wet end of the corrugator or by blade at the dry end of the corrugator.Description: Topical MVTR and water resistance coating Usage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include roll wrap, produce boxes, poultry boxes and anywhere packaged goods require protection from water and or moisture vapor. Application Data: VaporCoat® 330C is best applied by rod coater in-line or off-line at the wet end of the corrugator or by blade at the dry end of the corrugator. Common uses include: Roll wrap for fine papers; Multi-wall bags; Produce and poultry boxes; Frozen meat patty boxes; Archival storage; and Corrosion-sensitive products Information provided by Michelman® |