MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® VaporCoat® 330C Topical MVTR  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Topical MVTR and water resistance coating

Usage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include roll wrap, produce boxes, poultry boxes and anywhere packaged goods require protection from water and or moisture vapor.

Application Data: VaporCoat® 330C is best applied by rod coater in-line or off-line at the wet end of the corrugator or by blade at the dry end of the corrugator.Description: Topical MVTR and water resistance coating

Usage: VaporCoat® 330C is a repulpable, printable and cold set gluable moisture vapor coating. Common uses for VaporCoat® 330C include roll wrap, produce boxes, poultry boxes and anywhere packaged goods require protection from water and or moisture vapor.

Application Data: VaporCoat® 330C is best applied by rod coater in-line or off-line at the wet end of the corrugator or by blade at the dry end of the corrugator.

Common uses include: Roll wrap for fine papers; Multi-wall bags; Produce and poultry boxes; Frozen meat patty boxes; Archival storage; and Corrosion-sensitive products

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 - 1.23 g/cc1.21 - 1.23 g/cc
pH 8.0 - 9.08.0 - 9.0
Brookfield Viscosity 400 - 600 cP400 - 600 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceGray liquid
Solids TypePolymer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Rayon Acrypet® VH-001 Heat Stabilized PMMA

WMICHEL207 / 135124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.