MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Evonik ACEMATT® HK 450 Silica
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Properties and applications: ACEMATT 450 is an untreated coarse-grained precipitated silica, particularly suitable for pigmented coating systems. This highly efficient matting agent is used in can and coil coatings as well as decorative and industrial coatings.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 10.8 µm10.8 µmd50; ISO 13320-1
pH 6.06.05% in water; ISO 787-9
Specific Surface Area 500 m²/g500 m²/gISO 9277
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 98 %>= 98 %ISO 3262-19
 
Descriptive Properties
Content<1%Sulfate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sandvik Osprey SCM415 Low Alloy Steel Powder
NYC YT3WBHQ Y2O3 Powder for Spray Coating
JIS SCM435 Chromium Molybdenum Steel
BASF Pluracol® SG-450 Rigid Polyol

PEVONIM022 / 197226

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.