MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® PP CX03-82 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP CX03-82 is an emission optimised high crystalline copolymer. It offers high impact resistance, in perfect balance with high thermal dimensional stability, stiffness and flow. This for automotive interior applications UV-stabilised material has excellent aesthetic properties as well. It is the obvious alternative to connventional talc-filled copolymers, offering considerable weight saving advantage. SABIC® PP CX03-82 is a designated automotive grade. IMDS ID: 80775790

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inAll measurements on injection molded samples.; SABIC method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength, Yield 22.0 MPa3190 psiSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Yield 5.0 %5.0 %ISO 527-2 1A
Tensile Modulus 1.25 GPa181 ksiSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) NBNBISO 180/1A
 8.00 kJ/m²
@Temperature -20.0 °C
3.81 ft-lb/in²
@Temperature -4.00 °F
ISO 180/1A
 20.0 kJ/m²
@Temperature 0.000 °C
9.52 ft-lb/in²
@Temperature 32.0 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched NBNBISO 179/1eA
 NBNBISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 66.0 °C151 °Fat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 145 °C293 °Fat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentFalse
Emission<50 µg C/gVDA 277
Nucleating agentTrue
UV stabilizedTrue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11241 / 244708

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.