MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP CX03-82 PP (Global)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PP CX03-82 is an emission optimised high crystalline copolymer. It offers high impact resistance, in perfect balance with high thermal dimensional stability, stiffness and flow. This for automotive interior applications UV-stabilised material has excellent aesthetic properties as well. It is the obvious alternative to connventional talc-filled copolymers, offering considerable weight saving advantage. SABIC® PP CX03-82 is a designated automotive grade. IMDS ID: 80775790

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccISO 1183
Linear Mold Shrinkage 0.016 cm/cmAll measurements on injection molded samples.; SABIC method
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Tensile Strength, Yield 22.0 MPaSpeed of testing: 50 mm/min; ISO 527-2 1A
Elongation at Yield 5.0 %ISO 527-2 1A
Tensile Modulus 1250 MPaSpeed of testing: 1 mm/min; ISO 527-2 1A
Izod Impact, Notched (ISO) NBISO 180/1A
 8.00 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 20.0 kJ/m²
@Temperature 0.000 °C
ISO 180/1A
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched NBISO 179/1eA
 NBISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 66.0 °Cat 50 N (VST/B); Temperature rate: 120°C/h; ISO 306
 145 °Cat 10 N (VST/A); Temperature rate: 120°C/h; ISO 306
 
Descriptive Properties
Anti static agentFalse
Emission<50 µg C/gVDA 277
Nucleating agentTrue
UV stabilizedTrue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11241 / 244708

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.