MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Schmolz + Bickenbach 430FR Stainless Steel Bar
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Description: Ugitech’s 430FR is a ferritic stainless steel designed for soft magnetic components operating in corrosive environments. The 17.00% - 18.00% chromium makes corrosion resistance similar to 430F. The increased silicon content in this alloy allows increased magnetic characteristics over 430F in the annealed condition. 430FR has exhibited superior and consistent performance due to its higher electrical resistivity. The alloy was developed for applications that require a weak coercive magnetic force (Hc =1.88 – 3.00 Oe [150 – 240 A/m]) as needed in solenoid valves. Our controlled processing allows magnetic properties to be typically superior to industry norms. 430FR has an increased hardness over 430F, due to the increased silicon levels, reducing the deformation that occurs during the oscillation impacts that occur in AC and DC solenoid valves

Applications: Solenoid Valves and Injectors

Information provided by Schmolz + Bickenbach

Key Words: ASTM A838 Alloy 2; EN 10088-3 1.4105, X6CrMoS17
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.275 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 149 - 177Magnetically Annealed (Grade 1)
Tensile Strength 65.0 - 80.0 ksiMagnetically Annealed (Grade 1)
Tensile Strength, Yield 45.0 - 65.0 ksi
@Strain 0.2 %
Magnetically Annealed (Grade 1)
Elongation at Yield >= 25 %Magnetically Annealed (Grade 1)
Reduction of Area >= 40 %Magnetically Annealed (Grade 1)
Tensile Modulus 29700 ksi
 
Electrical PropertiesOriginal ValueComments
Magnetic Permeability 1200 - 2200[µ]
 2100[µ]; Typical delivered
Magnetic Coercive Force, Hc 2.3 Oe[µ]
 1.88 - 3.0 Oe[µ]; Typical delivered
Magnetic Saturation Flux Density, Bmax 16000 Gauss
Magnetic Remanence, Br 3000 - 7500 Gauss
 6700 GaussTypical delivered magnetic properties
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 20.0 - 200 °C
Thermal Conductivity 173 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 1292 - 1472 °F
@Time <=3600 sec
For softening
 1652 °F
@Time 7200 sec
Optimum magnetic properties; Then cool to 930°F at a rate of 120°F per hour
 1540 - 1830 °F
@Time 7200 sec
Then cool to 930°F at a rate of 120°F per hour
Hot-Working Temperature 1382 - 2192 °FUniformly heating
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.065 %
Chromium, Cr 17.25 - 18.25 %
Iron, Fe >= 77.855 %
Manganese, Mn <= 0.80 %
Molybdenum, Mo <= 0.50 %
Nickel, Ni <= 0.60 %
Phosphorus, P <= 0.030 %
Silicon, Si 1.0 - 1.5 %
Sulfur, S 0.25 - 4.0 %
 
Descriptive Properties
Corrosion ResistanceHumidity2/4
 NaCl 0.2g/l1.6% mass loss; 60°C; 500 hrs
 NaCl 0.4g/l1.6% mass loss; 60°C; 500 hrs
 NaCl 0.6g/l2.25% mass loss; 60°C; 500 hrs
 Sodium Carbonate2/4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type 430F Stainless Steel
AISI Type 430F Stainless Steel annealed bar
Crucible Steel 430F Stainless Steel
Carpenter Chrome Core® 18-FM Solenoid Quality Stainless Steel, Annealed
AISI Type 430F Stainless Steel annealed and cold drawn bar 25 mm diameter

NSCHMO038 / 125911

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.