MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 5002.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. LL 5002.09 also exhibits good toughness and environmental stress crack resistance.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Masterbatch Base Resin

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 39
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 1900 psiASTM D638
Tensile Strength, Yield 1700 psiASTM D638
Elongation at Break 730 %ASTM D638
Flexural Modulus, 1% Secant 40000 psiASTM D638
Izod Impact, Notched 8.90 ft-lb/inASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 252 °FPeak Melting Point; ExxonMobil method
Brittleness Temperature <= -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4340 Steel, annealed, 25 mm round
ExxonMobil C4LL 3625.85 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
ExxonMobil LL 5100.09 Compounding Resin
ExxonMobil LL 1002.09 Blown Film Resin

PEX99165 / 175401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.