MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LLDPE LL 1002YB Cast Linear Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: LL 1002YB is an LLDPE resin designed for cast films. It offers high gloss and excellent drawdown in both blown and cast film applications. LL 1002YB may also be used as a blend partner with LDPE resins to improve film properties and processability.

Availability: Africa & Middle East, Asia Pacific, Europe, Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Processing Aid: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Cast Stretch Film
  • Garment Film
  • General Packaging
  • Hygiene film
  • Packaging Films
  • Personal Care

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ExxonMobil method
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 7.58 MPa1100 psiASTM D882
Film Tensile Strength at Yield, TD 6.48 MPa940 psiASTM D882
Film Elongation at Break, MD 420 %420 %ASTM D882
Film Elongation at Break, TD 830 %830 %ASTM D882
Puncture Energy 2.37 J1.75 ft-lbExxonMobil Method
Elmendorf Tear Strength MD 20 g20 gASTM D1922
Elmendorf Tear Strength TD 430 g430 gASTM D1922
Dart Drop Test <= 50.0 g<= 0.110 lbASTM D1709A
Film Tensile Strength at Break, MD 62.1 MPa9000 psiASTM D882
Film Tensile Strength at Break, TD 24.8 MPa3600 psiASTM D882
1% Secant Modulus, MD 117 MPa17000 psiASTM D882
1% Secant Modulus, TD 131 MPa19000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point <= 120 °C<= 248 °FPeak Melting Point; ExxonMobil method
 
Optical PropertiesMetricEnglishComments
Haze 1.7 %1.7 %ASTM D1003
Gloss 98 %98 %45°; ASTM D2457
 
Descriptive Properties
Puncture Force8 lbfExxonMobil Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LLDPE LL 5002.09 Linear Low Density Polyethylene Resin
ExxonMobil C4LL 3625.85 Linear Low Density Polyethylene Resin
ExxonMobil C4LL 2018.YB Wire & Cable Linear Low Density Polyethylene Resin
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
ExxonMobil LLDPE LL 1002X75 Linear Low Density Polyethylene Resin

PEX99150 / 175386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.