MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eastman Eastar EN001 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming. Eastar EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.

Applications/Uses

  • Food Packaging
  • Housewares
  • Toys/Sporting goods
  • Writing instruments
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.33 g/ccISO 1183
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Rockwell R 112ASTM D785
     114ISO 2039-2
    Tensile Strength at Break 25.0 MPaISO 527
     25.0 MPaASTM D638
    Tensile Strength, Yield 57.0 MPaISO 527
     58.0 MPaASTM D638
    Elongation at Break 120 %ISO 527
     120 %ASTM D638
    Tensile Modulus 2.40 GPaISO 527
     2.40 GPaASTM D638
    Flexural Yield Strength 77.0 MPaISO 178
     84.0 MPaASTM D790
    Flexural Modulus 2.30 GPaISO 178
     2.50 GPaASTM D790
    Izod Impact, Notched 0.270 J/cm
    @Temperature -40.0 °C
    ASTM D256
     40.0 J/m
    @Temperature 23.0 °C
    ASTM D256
    Izod Impact, Unnotched NBASTM D4812
     NB
    @Temperature -40.0 °C
    ASTM D4812
    Izod Impact, Notched (ISO) 3.10 kJ/m²
    @Temperature -40.0 °C
    ISO 180
     4.50 kJ/m²
    @Temperature 23.0 °C
    ISO 180
    Izod Impact, Unnotched (ISO) NBISO 180
     170 kJ/m²
    @Temperature -40.0 °C
    ISO 180
    Puncture Energy 0.800 J
    @Thickness 2.50 mm,
    Temperature -40.0 °C
    max load; ISO 6603-2
     1.00 J
    @Thickness 3.20 mm,
    Temperature -40.0 °C
    max load; ISO 6603-2
     1.60 J
    @Thickness 2.50 mm,
    Temperature -40.0 °C
    max load; ASTM D3763
     2.10 J
    @Thickness 3.20 mm,
    Temperature -40.0 °C
    max load; ASTM D3763
     15.0 J
    @Thickness 2.50 mm,
    Temperature 23.0 °C
    max load; ISO 6603-2
     18.0 J
    @Thickness 3.20 mm,
    Temperature 23.0 °C
    max load; ISO 6603-2
     26.0 J
    @Thickness 2.50 mm,
    Temperature 23.0 °C
    max load; ASTM D3763
     31.0 J
    @Thickness 3.20 mm,
    Temperature 23.0 °C
    max load; ASTM D3763
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CISO 75
     69.0 °CASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 65.0 °CISO 75
     65.0 °CASTM D648
     
    Optical PropertiesOriginal ValueComments
    Haze 1.0 %ASTM D1003
    Transmission, Visible 84 %Total Transmittance; ASTM D1003
     
    Compliance PropertiesOriginal ValueComments
    FDA YesSee notes for details.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    PE9032 / 35088

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.