MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eastman Eastar EN001 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming. Eastar EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.

Applications/Uses

  • Food Packaging
  • Housewares
  • Toys/Sporting goods
  • Writing instruments
  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.33 g/cc0.0480 lb/in³ISO 1183
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell R 112112ASTM D785
     114114ISO 2039-2
    Tensile Strength at Break 25.0 MPa3630 psiISO 527
     25.0 MPa3630 psiASTM D638
    Tensile Strength, Yield 57.0 MPa8270 psiISO 527
     58.0 MPa8410 psiASTM D638
    Elongation at Break 120 %120 %ISO 527
     120 %120 %ASTM D638
    Tensile Modulus 2.40 GPa348 ksiISO 527
     2.40 GPa348 ksiASTM D638
    Flexural Yield Strength 77.0 MPa11200 psiISO 178
     84.0 MPa12200 psiASTM D790
    Flexural Modulus 2.30 GPa334 ksiISO 178
     2.50 GPa363 ksiASTM D790
    Izod Impact, Notched  0.270 J/cm
    @Temperature -40.0 °C
    0.506 ft-lb/in
    @Temperature -40.0 °F
    ASTM D256
     0.400 J/cm
    @Temperature 23.0 °C
    0.749 ft-lb/in
    @Temperature 73.4 °F
    ASTM D256
    Izod Impact, Unnotched NBNBASTM D4812
     NB
    @Temperature -40.0 °C
    NB
    @Temperature -40.0 °F
    ASTM D4812
    Izod Impact, Notched (ISO)  3.10 kJ/m²
    @Temperature -40.0 °C
    1.48 ft-lb/in²
    @Temperature -40.0 °F
    ISO 180
     4.50 kJ/m²
    @Temperature 23.0 °C
    2.14 ft-lb/in²
    @Temperature 73.4 °F
    ISO 180
    Izod Impact, Unnotched (ISO) NBNBISO 180
     170 kJ/m²
    @Temperature -40.0 °C
    80.9 ft-lb/in²
    @Temperature -40.0 °F
    ISO 180
    Puncture Energy  0.800 J
    @Thickness 2.50 mm,
    Temperature -40.0 °C
    0.590 ft-lb
    @Thickness 0.0984 in,
    Temperature -40.0 °F
    max load; ISO 6603-2
     1.00 J
    @Thickness 3.20 mm,
    Temperature -40.0 °C
    0.738 ft-lb
    @Thickness 0.126 in,
    Temperature -40.0 °F
    max load; ISO 6603-2
     1.60 J
    @Thickness 2.50 mm,
    Temperature -40.0 °C
    1.18 ft-lb
    @Thickness 0.0984 in,
    Temperature -40.0 °F
    max load; ASTM D3763
     2.10 J
    @Thickness 3.20 mm,
    Temperature -40.0 °C
    1.55 ft-lb
    @Thickness 0.126 in,
    Temperature -40.0 °F
    max load; ASTM D3763
     15.0 J
    @Thickness 2.50 mm,
    Temperature 23.0 °C
    11.1 ft-lb
    @Thickness 0.0984 in,
    Temperature 73.4 °F
    max load; ISO 6603-2
     18.0 J
    @Thickness 3.20 mm,
    Temperature 23.0 °C
    13.3 ft-lb
    @Thickness 0.126 in,
    Temperature 73.4 °F
    max load; ISO 6603-2
     26.0 J
    @Thickness 2.50 mm,
    Temperature 23.0 °C
    19.2 ft-lb
    @Thickness 0.0984 in,
    Temperature 73.4 °F
    max load; ASTM D3763
     31.0 J
    @Thickness 3.20 mm,
    Temperature 23.0 °C
    22.9 ft-lb
    @Thickness 0.126 in,
    Temperature 73.4 °F
    max load; ASTM D3763
     
    Thermal PropertiesMetricEnglishComments
    Deflection Temperature at 0.46 MPa (66 psi) 69.0 °C156 °FISO 75
     69.0 °C156 °FASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75
     65.0 °C149 °FASTM D648
     
    Optical PropertiesMetricEnglishComments
    Haze 1.0 %1.0 %ASTM D1003
    Transmission, Visible 84 %84 %Total Transmittance; ASTM D1003
     
    Compliance PropertiesMetricEnglishComments
    FDA YesYesSee notes for details.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PE9032 / 35088

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.