MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-SEAL® 6371 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.

Molded only

RoHS Compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.75 - 2.25 g/cc1.75 - 2.25 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 7555 - 75ASTM D2240
Tensile Strength at Break >= 1.03 MPa>= 150 psiASTM D412
Elongation at Break >= 100 %>= 100 %ASTM D412
Compression Set <= 40 %
@Temperature 100 °C,
Time 252000 sec
<= 40 %
@Temperature 212 °F,
Time 70.0 hour
ASTM D395 Method B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.10 ohm-cm0.10 ohm-cmwithout psa; CEPS-002
Shielding Effectiveness >= 100 dB>= 100 dB500 MHz (E Field); MIL-G-83528
 >= 80 dB
@Frequency 2.00e+9 Hz
>= 80 dB
@Frequency 2.00e+9 Hz
CHO-TM-TP08
 >= 80 dB
@Frequency 1e+9 Hz
>= 80 dB
@Frequency 1e+9 Hz
CHO-TM-TP08
 >= 100 dB
@Frequency 1e+8 Hz
>= 100 dB
@Frequency 1e+8 Hz
CHO-TM-TP08
 >= 100 dB
@Frequency 5.00e+8 Hz
>= 100 dB
@Frequency 5.00e+8 Hz
CHO-TM-TP08
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.10 W/m-K
@Pressure 2.07 MPa
7.63 BTU-in/hr-ft²-°F
@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °FFlex TR10; ASTM D1329
Flammability, UL94 V-0V-0
 
Descriptive Properties
BinderSilicone
FillerNi/C
Heat Aging<0.25 ohm-cm150°C for 48 hrs; CEPS-0002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-FORM 5537 EMI Shielding Material
Parker Chomerics CHO-SEAL 1356 Conductive Elastomer
Parker Chomerics CHO-SEAL L6303 Conductive Elastomer
Parker Chomerics CHO-SEAL® 6310 Extruded Elastomer
Parker Chomerics CHO-SEAL® 6370 Conductive Elastomer

PCHOME136 / 28358

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.