MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Thorium, Th
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.3 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 232.03811995
Atomic Number 90
X-ray Absorption Edge 0.1129 ÅK
 0.6061 ÅLI
 0.6301 ÅLII
 0.76151 ÅLIII
Electrode Potential -2.10 V
Electronegativity 1.3Pauling
Ionic Radius 1.02 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 35 - 114References report a wide range of values
Tensile Strength, Ultimate 219 MPaas cast; 0.02 to 0.08% C
Tensile Strength, Yield 144 MPa
@Strain 0.2 %
Elongation at Break 34 %
Modulus of Elasticity 73.1 GPa
Compressive Strength 220 MPaApproximately equal to tensile
Bulk Modulus 57.7 GPa
Poissons Ratio 0.27
Fatigue Strength 97.0 MPareversed bend test endurance limit
Shear Modulus 28.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000130 ohm-cm
Magnetic Susceptibility -1.10e-7cgs/g
Critical Magnetic Field Strength, Oersted 157 - 163
Critical Superconducting Temperature 1.36 - 1.40 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 82.9 J/g
Heat of Vaporization 2617 J/g
CTE, linear 11.1 µm/m-°C
@Temperature 20.0 °C
 12.6 µm/m-°C
@Temperature 600 °C
 14.9 µm/m-°C
@Temperature 950 °C
Specific Heat Capacity 0.09261 J/g-°C
@Temperature -193 °C
 0.09779 J/g-°C
@Temperature -173 °C
 0.1016 J/g-°C
@Temperature -153 °C
 0.1061 J/g-°C
@Temperature -113 °C
 0.1089 J/g-°C
@Temperature -73.0 °C
 0.1108 J/g-°C
@Temperature -23.0 °C
 0.1132 J/g-°C
@Temperature 27.0 °C
 0.1167 J/g-°C
@Temperature 127 °C
 0.1202 J/g-°C
@Temperature 227 °C
 0.1239 J/g-°C
@Temperature 327 °C
 0.1278 J/g-°C
@Temperature 427 °C
 0.132 J/g-°C
@Temperature 527 °C
 0.1364 J/g-°C
@Temperature 627 °C
 0.141 J/g-°C
@Temperature 727 °C
Thermal Conductivity 37.7 W/m-K
Melting Point 1800 °C
Boiling Point 4788 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 1127 °C
total spectrum
 
Component Elements PropertiesOriginal ValueComments
Thorium, Th 100 %
 
Descriptive Properties
CAS Number7440-29-1

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver, Ag
Thallium, Tl
Manganese, Mn
Terbium, Tb
Thulium, Tm

AMETh00 / 114

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.