MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Thorium, Th
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 11.3 g/cc0.408 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 232.0381232.03811995
Atomic Number 9090
X-ray Absorption Edge 0.1129 Å0.1129 ÅK
 0.6061 Å0.6061 ÅLI
 0.6301 Å0.6301 ÅLII
 0.76151 Å0.76151 ÅLIII
Electrode Potential -2.10 V-2.10 V
Electronegativity 1.31.3Pauling
Ionic Radius 1.02 Å1.02 ÅCrystal Ionic Radius for Valence +4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 35 - 11435 - 114References report a wide range of values
Tensile Strength, Ultimate 219 MPa31800 psias cast; 0.02 to 0.08% C
Tensile Strength, Yield 144 MPa
@Strain 0.2 %
20900 psi
@Strain 0.2 %
Elongation at Break 34 %34 %
Modulus of Elasticity 73.1 GPa10600 ksi
Compressive Strength 220 MPa31900 psiApproximately equal to tensile
Bulk Modulus 57.7 GPa8370 ksi
Poissons Ratio 0.270.27
Fatigue Strength 97.0 MPa14100 psireversed bend test endurance limit
Shear Modulus 28.0 GPa4060 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000130 ohm-cm0.0000130 ohm-cm
Magnetic Susceptibility -1.10e-7-1.10e-7cgs/g
Critical Magnetic Field Strength, Oersted 157 - 163157 - 163
Critical Superconducting Temperature 1.36 - 1.40 K1.36 - 1.40 K
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 82.9 J/g35.7 BTU/lb
Heat of Vaporization 2617 J/g1126 BTU/lb
CTE, linear  11.1 µm/m-°C
@Temperature 20.0 °C
6.17 µin/in-°F
@Temperature 68.0 °F
 12.6 µm/m-°C
@Temperature 600 °C
7.00 µin/in-°F
@Temperature 1110 °F
 14.9 µm/m-°C
@Temperature 950 °C
8.28 µin/in-°F
@Temperature 1740 °F
Specific Heat Capacity  0.09261 J/g-°C
@Temperature -193 °C
0.02213 BTU/lb-°F
@Temperature -315 °F
 0.09779 J/g-°C
@Temperature -173 °C
0.02337 BTU/lb-°F
@Temperature -279 °F
 0.1016 J/g-°C
@Temperature -153 °C
0.02428 BTU/lb-°F
@Temperature -243 °F
 0.1061 J/g-°C
@Temperature -113 °C
0.02536 BTU/lb-°F
@Temperature -171 °F
 0.1089 J/g-°C
@Temperature -73.0 °C
0.02603 BTU/lb-°F
@Temperature -99.4 °F
 0.1108 J/g-°C
@Temperature -23.0 °C
0.02648 BTU/lb-°F
@Temperature -9.40 °F
 0.1132 J/g-°C
@Temperature 27.0 °C
0.02705 BTU/lb-°F
@Temperature 80.6 °F
 0.1167 J/g-°C
@Temperature 127 °C
0.02789 BTU/lb-°F
@Temperature 261 °F
 0.1202 J/g-°C
@Temperature 227 °C
0.02873 BTU/lb-°F
@Temperature 441 °F
 0.1239 J/g-°C
@Temperature 327 °C
0.02961 BTU/lb-°F
@Temperature 621 °F
 0.1278 J/g-°C
@Temperature 427 °C
0.03054 BTU/lb-°F
@Temperature 801 °F
 0.132 J/g-°C
@Temperature 527 °C
0.0315 BTU/lb-°F
@Temperature 981 °F
 0.1364 J/g-°C
@Temperature 627 °C
0.03260 BTU/lb-°F
@Temperature 1160 °F
 0.141 J/g-°C
@Temperature 727 °C
0.0337 BTU/lb-°F
@Temperature 1340 °F
Thermal Conductivity 37.7 W/m-K262 BTU-in/hr-ft²-°F
Melting Point 1800 °C3270 °F
Boiling Point 4788 °C8650 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 1127 °C
0.30
@Temperature 2061 °F
total spectrum
 
Component Elements PropertiesMetricEnglishComments
Thorium, Th 100 %100 %
 
Descriptive Properties
CAS Number7440-29-1

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silver, Ag
Thallium, Tl
Manganese, Mn
Terbium, Tb
Thulium, Tm

AMETh00 / 114

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.