MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Skybond® 705 Aromatic Polyimide Resin for Coatings
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: SKYBOND® 705 is a heat reactive aromatic resin which can be thermally cured to a crosslinked polyimide with high heat resistance. It has good film forming properties useful for high temperature coating applications.

Information provided by Industrial Summit Technology Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.08 g/cc0.0379 - 0.0390 lb/in³
Solids Content 16 - 20 %16 - 20 %
Viscosity 1100 - 2600 cP1100 - 2600 cP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Skybond® 703 Aromatic Polyimide Resin for Composites
Skybond® 1028 Aromatic Polyimide Resin
Skybond® 875 Aromatic Polyimide Two Stage Resin
Skybond® 9100 Aromatic Polyimide Resin for RTM Molding
CEN® Electronic Material CTS Polyimide Resin

PISTEC953 / 183041

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.