MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CEN® Electronic Material CTS Polyimide Resin
Categories: Polymer; Film; Thermoset; Polyimide, TS

Material Notes: CEN® CTS polyimide resin is a high tensile strength, thermal stable, and viscose resin solution based on aromatic polyimide. The product offers high modulus value and high dimensional stability with lower coefficient thermal expansion (CTE) after cured. Nano size fillers can be dispersed with the resin for coating, and other specific applications, which changes the resin properties, such as thermal and electrical conductivity significantly.

Applications: fuser film sleeve for laser printer and copier, seamless tube, coating film, mechanical and electronic parts.

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 20 %20 %
Viscosity 80000 - 150000 cP80000 - 150000 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 320 MPa>= 46400 psi50µm coating

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 2237 Polyimide Resin System
Mitsui AURUM® PL450C Polyimide
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
Arlon Electronic Materials 85N Polyimide Laminate and Prepreg
Mitsubishi Chemical Advanced Materials Duratron® D7000 PI Unfilled Polyimide (ASTM Product Data Sheet)

PCENE001 / 93463

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.