MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos Styrenics 473D High-Impact Polystyrene Resin (NAFTA)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description: High-impact, high-flow grade for a wide variety of applications, including appliance components, consumer electronics housings, magnetic and optical media, building and construction, packaging and food service, recreation equipment and sporting goods, medical devices and labware, office products, cosmetic and personal care products, and housewares.

Information provided by BASF.


Ineos Styrenics purchased this product line from BASF in 2005.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792
Water Absorption at Saturation <= 0.10 %
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmASTM D955
Melt Flow 13 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 16.0 MPaASTM D638
Tensile Strength, Yield 21.0 MPaASTM D638
Elongation at Break 60 %ASTM D638
Tensile Modulus 2.275 GPaASTM D638
Flexural Modulus 1.98 GPaASTM D790-1
Izod Impact, Notched 2.10 ft-lb/inASTM D256-A
Gardner Impact 250 in-lb
@Temperature 23.0 °C
ASTM D5420, GB
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 81.1 °CASTM D648
Vicat Softening Point 93.3 °CASTM D1525
Flammability, UL94 HB
@Thickness 1.50 mm
Natural Color
 
Optical PropertiesOriginal ValueComments
Gloss 55 %60°; ASTM D523
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 280 °CInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos Nova 5511 High Impact Polystyrene
Lotte Advanced Materials Starex® HF-0690M ABS, Unreinforced
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene
Ineos Styrenics Polystyrene 486N (NAFTA)
Ineos Styrenics Polystyrene 476M (NAFTA)

PSG102 / 67263

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.