MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C66400, H10 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes:

Applications: spring washers, switchblades, fuse clips, contact springs, socket contacts, connectors, terminals.

Key Words: Cobron
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.74 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 690 MPa100000 psi
Tensile Strength, Yield 640 MPa
@Strain 0.2 %
92800 psi
@Strain 0.2 %
Elongation at Break 3.0 %3.0 %in 50 mm
Modulus of Elasticity 112 GPa16200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000575 ohm-cm
@Temperature 20.0 °C
0.00000575 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 116 W/m-K805 BTU-in/hr-ft²-°F
Melting Point 1035 - 1055 °C1895 - 1931 °F
Solidus 1035 °C1895 °F
Liquidus 1055 °C1931 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.050 %<= 0.050 %
Cobalt, Co 0.30 - 0.70 %0.30 - 0.70 %
Copper, Cu 86.5 %86.5 %
Iron, Fe 1.3 - 1.7 %1.3 - 1.7 %
Lead, Pb <= 0.015 %<= 0.015 %
Manganese, Mn <= 0.050 %<= 0.050 %
Nickel, Ni <= 0.050 %<= 0.050 %
Phosphorus, P <= 0.020 %<= 0.020 %
Silicon, Si <= 0.050 %<= 0.050 %
Silver, Ag <= 0.050 %<= 0.050 %
Tin, Sn <= 0.050 %<= 0.050 %
Zinc, Zn 11 - 12 %11 - 12 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C40800
Copper, UNS C15720, 0.152 mm thick flat product, 98% Cold Worked
Copper, UNS C15720
Copper nickel 20%, UNS C71000, H55 Temper flat products
Copper nickel 20%, UNS C71000, H04 Temper flat products

MC66400b8 / 11678

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.