MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper, UNS C15720
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Excellent cold workability. Fabricated by extrusion, drawing, rolling, impacting, heading, swaging, bending, machining, blanking.

Applications: relay and switch springs, lead frames, contact supports, heat sinks, circuit breaker parts, rotor bars, resistance welding electrodes and wheels, connectors, high strength high temperature parts.

Available as flat products and rod.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.81 g/cc0.318 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 462 - 614 MPa67000 - 89100 psi
Tensile Strength, Yield 365 - 586 MPa52900 - 85000 psiDepending on temper
Elongation at Break 20 %20 %in 88.9 mm.
Modulus of Elasticity 113 GPa16400 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000190 ohm-cm0.00000190 ohm-cm89% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.6 µm/m-°C
@Temperature 20.0 - 300 °C
10.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.377 J/g-°C0.0900 BTU/lb-°F
Thermal Conductivity 353 W/m-K2450 BTU-in/hr-ft²-°F
Melting Point <= 1080 °C<= 1980 °F
Solidus 1083 °C1981 °F
Liquidus 1080 °C1980 °F
Annealing Point 649 - 982 °C1200 - 1800 °F
 
Component Elements PropertiesMetricEnglishComments
Al2O3 0.35 - 0.45 %0.35 - 0.45 %
Copper, Cu 99.49 - 99.6 %99.49 - 99.6 %Specified
Iron, Fe <= 0.010 %<= 0.010 %
Lead, Pb <= 0.010 %<= 0.010 %
Oxygen, O <= 0.040 %<= 0.040 %Excluding Al2O3

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, UNS C12000
Copper, UNS C15710
Copper, UNS C15760
Beryllium Copper, UNS C17000
Cadmium-Copper, Deoxidized, UNS C14310

MC15720b1 / 10682

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.