MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Extrusion Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.24 - 1.40 g/ccAverage value: 1.32 g/cc Grade Count:24
Water Absorption 0.0800 - 0.450 %Average value: 0.207 % Grade Count:6
Moisture Absorption at Equilibrium 0.0800 - 0.200 %Average value: 0.133 % Grade Count:6
Linear Mold Shrinkage 0.00160 - 0.0230 cm/cmAverage value: 0.0140 cm/cm Grade Count:12
Linear Mold Shrinkage, Transverse 0.00160 - 0.0170 cm/cmAverage value: 0.0125 cm/cm Grade Count:7
Melt Flow 8.00 - 236 g/10 minAverage value: 44.6 g/10 min Grade Count:12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 79.0 - 119Average value: 108 Grade Count:5
Tensile Strength, Ultimate 48.0 - 68.0 MPaAverage value: 55.5 MPa Grade Count:17
Tensile Strength, Yield 40.0 - 60.0 MPaAverage value: 53.5 MPa Grade Count:8
Elongation at Break 2.90 - 300 %Average value: 81.6 % Grade Count:23
Elongation at Yield 2.90 - 4.50 %Average value: 3.75 % Grade Count:6
Modulus of Elasticity 1.75 - 2.86 GPaAverage value: 2.53 GPa Grade Count:8
Flexural Yield Strength 70.0 - 94.0 MPaAverage value: 78.9 MPa Grade Count:11
Flexural Modulus 0.196 - 2.55 GPaAverage value: 2.06 GPa Grade Count:17
Izod Impact, Notched 0.0400 - 0.800 J/cmAverage value: 0.543 J/cm Grade Count:11
Izod Impact, Notched (ISO) 7.00 - 7.00 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 7.00 kJ/m² Grade Count:1
Izod Impact, Unnotched (ISO) NB - NB
@Temperature -30.0 - -30.0 °C
Grade Count:1
Charpy Impact Unnotched 15.0 J/cm² - NBAverage value: 15.0 J/cm² Grade Count:4
 22.0 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 22.0 J/cm² Grade Count:4
Charpy Impact, Notched 0.160 - 1.00 J/cm²Average value: 0.433 J/cm² Grade Count:9
 0.500 - 1.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.700 J/cm² Grade Count:3
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 - 1.00e+16 ohm-cmAverage value: 5.83e+15 ohm-cm Grade Count:6
Surface Resistance 1.00e+14 - 1.00e+15 ohmAverage value: 7.00e+14 ohm Grade Count:3
Dielectric Constant 3.10 - 3.70Average value: 3.37 Grade Count:7
Dielectric Strength 15.7 - 28.0 kV/mmAverage value: 23.1 kV/mm Grade Count:8
Dissipation Factor 0.00100 - 0.0200Average value: 0.0108 Grade Count:4
Arc Resistance 110 - 180 secAverage value: 130 sec Grade Count:4
Comparative Tracking Index 600 VAverage value: 600 V Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 130 µm/m-°CAverage value: 85.9 µm/m-°C Grade Count:11
CTE, linear, Transverse to Flow 70.0 - 130 µm/m-°CAverage value: 95.0 µm/m-°C Grade Count:5
Melting Point 215 - 254 °CAverage value: 226 °C Grade Count:15
Deflection Temperature at 0.46 MPa (66 psi) 60.0 - 170 °CAverage value: 137 °C Grade Count:11
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 170 °CAverage value: 65.2 °C Grade Count:20
Vicat Softening Point 130 - 216 °CAverage value: 199 °C Grade Count:5
Flammability, UL94 HB - V-2Grade Count:17
 
Processing PropertiesOriginal ValueComments
Processing Temperature 230 - 260 °CAverage value: 246 °C Grade Count:5
Melt Temperature 250 - 270 °CAverage value: 260 °C Grade Count:5
Mold Temperature 60.0 - 100 °CAverage value: 80.0 °C Grade Count:9
Drying Temperature 80.0 - 120 °CAverage value: 105 °C Grade Count:6

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant

O3201 / 78166

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.