MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Phosphor Bronze, UNS C94400, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Continuous, and Sand.

Applications: General-utility alloy for bushings and bearings.

Classified under: High-leaded tin bronzes. ASTM B66

As cast values below are for sand casting. Alloy does not respond to heat treating

Key Words: Leaded phosphor bronze, ASTM B66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.08 g/ccEstimated
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 55500 kg
Tensile Strength, Ultimate 221 MPaas cast
Tensile Strength, Yield 110 MPaas cast
Elongation at Break 18 %as cast
Machinability 80 %UNS C36000 (free-cutting brass) = 100%
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 81 %
Lead, Pb 11 %
Tin, Sn 8.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
Leaded Nickel Tin Bronze, UNS C94800, Copper Casting Alloy
Copper, UNS C62400 (Aluminum Bronze 11%)
Medium Bronze, UNS C94500, Copper Casting Alloy

MC94400b1 / 11956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.