MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Medium Bronze, UNS C94500, Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal and Sand.

Applications: Locomotive wearing parts, high-speed low-load bearings.

Classified under: High-leaded tin bronzes. ASTM B66

Alloy does not respond to heat treating

Key Words: High lead tin bronze, ASTM B66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 9.40 g/cc0.340 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 5050
Tensile Strength, Ultimate 170 MPa24700 psi
Tensile Strength, Yield 83.0 MPa12000 psi
Elongation at Break 12 %12 %in 50 mm
Modulus of Elasticity 72.0 GPa10400 ksi
Compressive Strength 250 MPa36300 psi
Fatigue Strength 69.0 MPa
@# of Cycles 1.00e+8
10000 psi
@# of Cycles 1.00e+8
rotating beam
Machinability 80 %80 %UNS C36000 (free-cutting brass) = 100%
Izod Impact 5.40 J3.98 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000017241 ohm-cm
@Temperature 20.0 °C
0.000017241 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.01.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.5 µm/m-°C
@Temperature 20.0 - 200 °C
10.3 µin/in-°F
@Temperature 68.0 - 392 °F
Specific Heat Capacity 0.376 J/g-°C0.0899 BTU/lb-°F
Thermal Conductivity 52.0 W/m-K
@Temperature 20.0 °C
361 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 315 °C599 °FIncipient
 800 - 940 °C1470 - 1720 °F
Solidus 800 °C1470 °F
Liquidus 940 °C1720 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.0050 %<= 0.0050 %
Antimony, Sb <= 0.80 %<= 0.80 %
Copper, Cu 73 %73 %
Iron, Fe <= 0.15 %<= 0.15 %
Lead, Pb 16 - 22 %16 - 22 %
Nickel, Ni <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.50 %<= 0.50 %
Silicon, Si <= 0.0050 %<= 0.0050 %
Sulfur, S <= 0.080 %<= 0.080 %
Tin, Sn 6.0 - 8.0 %6.0 - 8.0 %
Zinc, Zn <= 1.2 %<= 1.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
High-Leaded Tin Bronze, UNS C93900, Copper Casting Alloy
High-Leaded Tin Bronze, UNS C94300, Copper Casting Alloy
Leaded Phosphor Bronze, UNS C94400, Copper Casting Alloy
Leaded Nickel Tin Bronze, UNS C94800, Copper Casting Alloy
Nickel Tin Bronze, UNS C94700, Copper Casting Alloy

MC94500b1 / 11957

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.