MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Saint-Gobain Tygon® E-70-V-CE Taste Barrier Tubing Formulation  (discontinued **)
Categories: Polymer

Material Notes: Formerly Vendflow® E-70-V-CE. Non-plasticized inner bore yeilds no taste: Vendflow® E-70-V-CE is formulated to transfer water and beverages without imparting any "plastic" taste sometimes found in PVC tubing. It is produced with a smooth, plasticizer free, hydrophobic inner surface to help maintain fluid purity. It meets FDA requirements for food contact, ensuring the safety of the user. Vendflow® E-70-V-CE is made for the food and beverage industries. It's exceptionally flexible, allowing for tight bends and easy installation on dispensing units. Its special construction will ensure a long tubing life, lessening the need for constant replacement.

Features/Benefits:
  • Plasticizer free fluid pathway
  • No taste
  • Smooth inner surface
  • Extremely low absorption rate
  • Custom colors, sizes, and lengths
  • High clarity
  • Meets FDA requirements for food contact
  • Hydrophobic inner surface reduces taste transfer
FDA approved for food contact.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792-00
Water Absorption <= 0.010 %<= 0.010 %24 hours at 23°C; ASTM D570-98
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 7767 - 77ASTM D2240
Tensile Strength, Yield 15.9 MPa2300 psiASTM D-412-98
Elongation at Break 240 %240 %ASTM D-412-98
Flexural Strength 1.38 MPa200 psi5/16" ID x 7/16" OD; ASTM D1599
 1.41 MPa205 psi1/4" ID x 3/8" OD; ASTM D1599
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 71.1 °C160 °F
Brittleness Temperature -43.9 °C-47.0 °FASTM D746-98
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ506 / 69020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.