MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stability

Colors: it is supplied in natural color and black color.

Available in: Latin America and North America

Main Properties: ? Dimensional stability, Impact Resistance, Stiffness, and Excellent thermal resistance

Applications: TECHNYL C 218 V50 is indicated for pieces that require dimensional stability and good mechanical proprieties like impact at higher temperatures.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183/A
Water Absorption 0.75 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 225 MPaISO R 527
Elongation at Break 2.0 %ISO R 527
Tensile Modulus 14600 MPaISO R 527
Izod Impact, Notched (ISO) 17.0 kJ/m²ISO 180
Charpy Impact Unnotched 107 kJ/m²ISO 179
Charpy Impact, Notched 19.0 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmCEI 93
Dielectric Constant 3.8CEI 250
Dissipation Factor 0.020CEI 250
Comparative Tracking Index 550 VCEI 112
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75/Af
Flammability, UL94 HB
@Thickness 0.400 mm
Oxygen Index 23 %ISO 4589
Glow Wire Test 650 °C
@Thickness 1.60 mm
CEI 695
 
Processing PropertiesOriginal ValueComments
Feed Temperature 225 - 230 °C
Nozzle Temperature 230 - 240 °C
Mold Temperature 80.0 - 100 °C
 
Descriptive Properties
Compression Zone230-240°C
Mixing Zone240-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, Conditioned
Domo TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Domo TechnylStar™ AFX 218 V50 PA6, 50% glass filled
Domo TechnylStar™ SX 216 V50 PA6, 50% glass filled, DRY

PRHOD773 / 138004

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.