MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ITW Densit® DENSIPHALT® Grout
Categories: Ceramic

Material Notes: Densiphalt® consists of an open-graded asphalt, with the voids filled with a high-strength cement-based mortar. Densiphalt® is applied as a 30-100 mm layer, and is laid on an adequate base course such as asphalt, CBM/cement stabilized gravel or standard concrete. Densiphalt® can be colored in a variety of shades. SPECIFICATION: • The base course is sealed with bitumen emulsion. • The open-graded asphalt is laid (special recipe). Then the dry Densiphalt® mortar is mixed with water in a special continuous flow mixer • The open-graded asphalt is filled with Densiphalt® mortar and the surface is finished with a rubber scraper. • Finally, the surface is sealed with Densit® Curing Compound.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 - 2.25 g/cc0.0797 - 0.0814 lb/in³Mortar; EN 12190
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 8.00 - 12.0 GPa1160 - 1740 ksiMortar and Asphalt; Dynamic; ASTM D4123
Flexural Strength 7.00 MPa1020 psiEN 196. 1 day. Mortar
 12.0 MPa1740 psiEN 196. 7 day. Mortar
 15.0 MPa2180 psiEN 196. 28 days. Mortar
Compressive Strength 4.00 - 7.00 MPa580 - 1020 psi1 day. Densiphalt® asphalt with 8/11 crushed aggregate; Mortar and Asphalt
 7.00 - 10.0 MPa1020 - 1450 psi7 day. Densiphalt® asphalt with 8/11 crushed aggregate; Mortar and Asphalt
 8.00 - 12.0 MPa1160 - 1740 psi28 day. Densiphalt® asphalt with 8/11 crushed aggregate; Mortar and Asphalt
 50.0 MPa7250 psiEN 12190. 1 day. Mortar
 80.0 MPa11600 psiEN 12190. 7 days. Mortar
 110 MPa16000 psiEN 12190. 28 days. Mortar
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.5 µm/m-°C6.94 µin/in-°F
 
Descriptive Properties
Chromate, Cr6+ Content (%)<0.0002
Fire ClassificationA1EN 13501-1. Mortar.
 A2, -S1EN 13501-1. Mortar and Asphalt
Freeze Thaw Resistance (kg/m2)<0.1CEN TS 12390-9. Mortar and Asphalt
Slip Resistance50 to 60 SRTBS 812. Standard surface. Mortar and Asphalt
 80 SRTBS 812. Shot-blasted surface. Mortar and Asphalt
Wear Resistance (cm3/50 cm2)7 to 8En 13892-3. Dependent of aggregate type. Mortar and Asphalt

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWDE9078 / 239588

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.