Densiphalt® consists of an open-graded asphalt, with the voids filled with a high-strength cement-based mortar. Densiphalt® is applied as a 30-100 mm layer, and is laid on an adequate base course such as asphalt, CBM/cement stabilized gravel or standard concrete. Densiphalt® can be colored in a variety of shades. SPECIFICATION: • The base course is sealed with bitumen emulsion. • The open-graded asphalt is laid (special recipe). Then the dry Densiphalt® mortar is mixed with water in a special continuous flow mixer • The open-graded asphalt is filled with Densiphalt® mortar and the surface is finished with a rubber scraper. • Finally, the surface is sealed with Densit® Curing Compound.Information provided by ITW Performance Polymers. |