MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Isoflon PUR Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes:
  • Very high wear resistance
  • Highly resilient

Information provided by Isoflon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccDIN 53479
Water Absorption 0.30 - 0.50 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D785
Hardness, Shore D 60DIN 53505
Tensile Strength 0.300 - 0.390 MPaDIN 53455
Elongation at Break 200 - 800 %DIN 53455
Tensile Modulus 8.00 - 700 MPaDIN 53457
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.4 - 7.1
@Frequency 1000 Hz
DIN 53483
Dielectric Strength 14.0 - 26.0 kV/mmDIN 53481
 
Thermal PropertiesOriginal ValueComments
CTE, linear 160 - 190 µm/m-°CDIN 52328
Thermal Conductivity 0.290 W/m-KDIN 52612
Maximum Service Temperature, Air 80.0 °CContinuous; DIN 52612
Minimum Service Temperature, Air -70.0 °CContinuous; DIN 52612
 
Descriptive Properties
ColorSeveral Colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 5154-H112
Covestro Baydur® GS PUR Polyurethane
BASF Ultraform® N2640 Z2 POM + PUR
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified

PISOFL925 / 123313

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.