MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow SE BR-1202C Stereospecific high cis-1,4 Polybutadiene (BR)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: SE BR-1202C is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low level of impurities. A non-staining stabilizer is added during the production process. It complies with the compositional requirements of the food packaging regulations of European countries and the USA. BR-1202C is uses for the manufacture of toughened polystyrene employing grafting processes. BR-1202C is supplied in bales weighing ca. 34 kg. Bales are wrapped in 60 micron PS film.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 57 cPiin 5% mass in styrene solution; Supplier Method
Ash 0.030 %ASTM D1416
Collected Volatile Condensable Material 0.20 %ASTM D1416
Storage Temperature <= 30.0 °C
ASTM Color 5.0[APHA]; in 5% mass styrene solution; ASTM D1209
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
 
Descriptive Properties
Cis-1,4 Content %97Supplier Method (NMR)
Dry Gel Content mg/kg50Supplier Method
Stabilizer wt%0.25non-staining
Wet Gel Index2Supplier Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SE BR-1202D Stereospecific high cis-1,4 Polybutadiene (BR)
Synthos BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220L Stereospecific high cis-1,4 Polybutadiene (BR)
Dow SE BR-1220M Stereospecific high cis-1,4 Polybutadiene (BR)

PDOW1095 / 30299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.