Vydyne R413H NT is general-purpose, heat-stabilized, impact-modified, 15% glass-fiber reinforced PA66 resin. It is specifically designed to maximize toughness, while retaining physical properties. This product is also lubricated for improved flow and offers superior surface appearance.Information provided by Ascend Performance Materials. |