MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ascend Performance Materials Vydyne® R413H BK07 Impact Modified Nylon 66, 13% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Vydyne R413H BK07 is general-purpose, heat-stabilized, impact-modified, 15% glass-fiber reinforced PA66 resin. Available in black, It is specifically designed to maximize toughness, while retaining physical properties. This product is also lubricated for improved flow and offers superior surface appearance.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³DAM; ISO 1183
Water Absorption 1.0 %
@Time 86400 sec
1.0 %
@Time 24.0 hour
DAM; ISO 62
Moisture Absorption at Equilibrium 1.9 %1.9 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 2.00 mm
0.0070 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
@Thickness 2.00 mm
0.0080 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 80.0 MPa11600 psi50% RH; ISO 527-2
 110 MPa16000 psiDAM; ISO 527-2
Elongation at Break 5.0 %5.0 %DAM; ISO 527-2
 13 %13 %50% RH; ISO 527-2
Tensile Modulus 4.10 GPa595 ksi50% RH; ISO 527-2
 5.50 GPa798 ksiDAM; ISO 527-2
Flexural Strength 73.0 MPa10600 psi50% RH; ISO 178
 140 MPa20300 psiDAM; ISO 178
Flexural Modulus 2.80 GPa406 ksi50% RH; ISO 178
 4.80 GPa696 ksiDAM; ISO 178
Poissons Ratio 0.400.40ISO 527-2
Izod Impact, Notched (ISO)  9.00 kJ/m²
@Temperature -40.0 °C
4.28 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 9.00 kJ/m²
@Temperature -40.0 °C
4.28 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 21.0 kJ/m²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  7.00 J/cm²
@Temperature -30.0 °C
33.3 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 7.60 J/cm²
@Temperature 23.0 °C
36.2 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.500 J/cm²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 0.500 J/cm²
@Temperature -40.0 °C
2.38 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm
@Thickness 1.00 mm
1.00e+11 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Dielectric Strength 3.00 kV/mm
@Thickness 1.00 mm
76.2 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
60 - 120 sec
@Thickness 0.118 in
PLC 6; ASTM D 495
Comparative Tracking Index 400 - 599 V
@Thickness 3.00 mm
400 - 599 V
@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
 7.0 - 15 sec7.0 - 15 secPLC 4; UL 746
High Amp Arc Ignition, HAI 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
 60 - 120 arcs60 - 120 arcsPLC 1; UL 746
High Voltage Arc-Tracking Rate, HVTR 80.0 - 150 mm/min3.15 - 5.91 in/minPLC 3; UL 746
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
16.7 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
61.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 258 °C496 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 235 °C455 °FUnannealed; DAM; ISO 75-2/A
UL RTI, Electrical  120 °C
@Thickness 0.400 mm
248 °F
@Thickness 0.0157 in
UL 746
 130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
UL 746
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
UL 746
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact  85.0 °C
@Thickness 0.400 mm
185 °F
@Thickness 0.0157 in
UL 746
 85.0 °C
@Thickness 0.750 mm
185 °F
@Thickness 0.0295 in
UL 746
 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact  125 °C
@Thickness 0.400 mm
257 °F
@Thickness 0.0157 in
UL 746
 125 °C
@Thickness 0.750 mm
257 °F
@Thickness 0.0295 in
UL 746
 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
Agency RatingsASTM, D4066 PA016G15
 ASTM, D6779 PA016G15
AppearanceBlack
Automotive Material SpecificationDelphi M2279V
FeaturesChemical Resistant
 Creep Resistant
 Gasoline Resistant
 Good Dimensional Stability
 Good Flow
 Good Impact Strength
 Good Mold Release
 Grease Resistant
 High Rigidity
 High Strength
 High Tensile Strength
 Impact Modified
 Lubricated
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
Ascend Performance Materials Vydyne® R413H NT Impact Modified Nylon 66, Glass Filled
Ravago Manufacturing Americas Enviramid N1315THL BK Nylon 66, 15% Glass Filled, Impact Modified, DAM
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6
Ravago Manufacturing Americas Hylon® N1013HL Nylon 6/6 (Cond)

PASCE9717 / 220820

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.