MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Metech 3541 Platinum Silver Conductor Composition
Categories: Polymer; Adhesive

Material Notes: These conductor compositions employ a state of the art mixed bond frit system to enhance adhesion and conductivity values while offering a range of cost effective conductors compatible with most resistor and dielectric systems.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 180000 - 220000 cP
@Temperature 25.0 °C
180000 - 220000 cP
@Temperature 77.0 °F
HBT, Spindle #SC4-14 @ 10rpm
Thickness 12.0 - 14.0 microns0.472 - 0.551 milFired
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 0.0070 ohm0.0070 ohm
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
Adhesion3-4lbs; aged
 7-8lbs; initial
Coverage (cm²/gm)70-75Calculated from 50 micron wet film
Line Resolution (microns)125
Solder Leach Resistance (5 sec. cycles)5Cycles required to leach 50% of a 10 mil wide conductive line using 62Sn/36Pb/2Ag at 230ºC
Solder Wetting (seconds)< 3Time required to 100% solder wet 0.08" x 0.08" pad size using 62Sn/36Pb/2Ag at 230ºC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4140 Steel, normalized at 870°C (1600°F), reheated to 845°C (1550°F), oil quenched, 315°C (600°F) temper, 25 mm (1 in.) round
Lord Adhesives Metech 3540 Platinum Silver Conductor Composition
Lord Adhesives Metech 3524D Silver Conductor Composition
Lord Adhesives Metech 3524 Silver Conductor Composition
Lord Adhesives Metech 3505 Palladium Silver Conductor Composition

PLORD079 / 86087

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.