Designation ISO 1874-PA11,EHLS,18-010,CD10 Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized. No need of lubricant. Low friction coefficient. Good abrasion resistance. High chemical resistance. Example applications: Control cable tubing. Information provided by Arkema. |