MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Arkema Rilsan® BESN G9 TL Nylon 11, Graphite Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11 with Graphite Filler

Material Notes: Designation ISO 1874-PA11,EHLS,18-010,CD10

Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.

No need of lubricant. Low friction coefficient. Good abrasion resistance. High chemical resistance.

Example applications: Control cable tubing.

Information provided by Arkema.

Key Words: PA11; Polyamide 11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
 1.09 g/cc0.0394 lb/in³Cond.; ISO 1183
Water Absorption 1.7 %1.7 %Dry; Sim. to ISO 62
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 235 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 71
@Time 15.0 sec
71
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength, Yield 46.0 MPa6670 psiCond.; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Cond.; ISO 527-1/-2
Tensile Modulus 2.13 GPa309 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 0.700 J/cm²
@Temperature 23.0 °C
3.33 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+13 ohm-cm5.00e+13 ohm-cmCond.; IEC 60093
Surface Resistance 6.00e+13 ohm6.00e+13 ohmCond.; IEC 60093
Dielectric Strength 55.0 kV/mm1400 kV/inCond.; IEC 60243-1
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 186 °C367 °F10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 168 °C334 °FDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C133 °FDry; ISO 75-1/-2
Vicat Softening Point 162 °C324 °F50°C/h 50N; Dry; ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °FInjection Molding; ISO 294
Mold Temperature 50.0 °C122 °FInjection Molding; ISO 10724
Hold Pressure 16.0 MPa2320 psiInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based85ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
LubricantsYes
Moisture SensitiveYes
Processing MethodsFilm Extrusion
 Injection Molding
 Other Extrusion
 Profile Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESN Y T6L PA12-Z2
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Arkema Rilsan® 8020 Nylon 11, Flexible Tubing Grade
A. Schulman ComAlloy Hiloy® 653 Nylon 6/6, Carbon Fiber Reinforced, Flow Enhanced

PARKG614 / 25866

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.