MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 157CW Wire & Cable Low Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 157CW is a medium density LDPE recommended for the production of Low Voltage power cable insulation, using the on-step silane cross0linking technology. The grade contains a higher level of antioxidants. Sufficient Cu-inhibitor should be added to meet specific ageing requirements.

Availability: Africa & Middle East and Europe

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • LV silane cross-linkable insulation – 1 step process
  • Telecom/Data/LAN cable insulation

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.931 g/ccExxonMobil method
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 54
@Time 15.0 sec
ASTM D2240
Tensile Strength at Break 2300 psiASTM D638
Tensile Strength, Yield 2000 psiASTM D638
Elongation at Break 550 %ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus, 1% Secant 52000 psiASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+15 ohm-cmASTM D257
Dielectric Constant 2.2ASTM D150
Dielectric Strength 1500 V/milASTM D149
Dissipation Factor 0.0010ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 239 °FPeak Melting Point; ExxonMobil method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil LDPE LD 103.59 Low Density Polyethylene Resin
ExxonMobil LDPE LD 103.09 Low Density Polyethylene Resin
ExxonMobil LDPE LD 102.LC Low Density Polyethylene Resin
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin

PEX99267 / 175503

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.