MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 100 PPH 155 FR Z2568 Polypropylene (PP); Flame Retardant - Preliminary Datasheet
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccISO 1183
Linear Mold Shrinkage 0.014 - 0.020 cm/cm
@Thickness 4.00 mm
0.014 - 0.020 in/in
@Thickness 0.157 in
ISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 32.0 MPa4640 psiISO 527
Elongation at Break >= 10 %>= 10 %ISO 527
Tensile Modulus 1.50 GPa218 ksiISO 527
Flexural Strength 40.0 MPa5800 psiISO 178
Flexural Modulus 1.60 GPa232 ksiISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Thickness 4.00 mm
1.43 ft-lb/in²
@Thickness 0.157 in
ISO 180/1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
@Thickness 4.00 mm
42.8 ft-lb/in²
@Thickness 0.157 in
ISO 180/1U
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 30.0 - 65.0 °C86.0 - 149 °F
Drying Temperature 80.0 °C
@Time 7200 sec
176 °F
@Time 2.00 hour
Injection Pressure 70.0 - 105 MPa10200 - 15200 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant
RTP Company RTP 199 X 138253 A Polypropylene (PP); Flame Retardant - High Impact - UV Stabilized
Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
RTP Company RTP 199 X 137777 Polypropylene (PP) Flame Retardant
RTP Company RTP 199 X 143560 B Polypropylene (PP); Flame Retardant - Halogen Free - Preliminary Datasheet

PQZRA35990 / 206100

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.