Compound 3525 is a 50 durometer white colored Buna N elastomer. It exhibits good resistance to heat and compression set. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BG 504 B14 B34 EO14 EA14; 5 BG 504 A14 B14 B34 EO14 CFR21 177.2600 Information provided by Pressure Seals Inc. |