MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pressure Seal 3525 Nitrile - Butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 3525 is a 50 durometer white colored Buna N elastomer. It exhibits good resistance to heat and compression set.

This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BG 504 B14 B34 EO14 EA14; 5 BG 504 A14 B14 B34 EO14
CFR21 177.2600

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5353
 39
@Treatment Temp. 100 °C,
Time 252000 sec
39
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 39
@Treatment Temp. 23.0 °C,
Time 252000 sec
39
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 40
@Treatment Temp. 100 °C,
Time 252000 sec
40
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 50
@Treatment Temp. 23.0 °C,
Time 252000 sec
50
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 51
@Treatment Temp. 100 °C,
Time 252000 sec
51
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 51
@Treatment Temp. 100 °C,
Time 252000 sec
51
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
Tensile Strength 5.25 MPa762 psi
 1.85 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
269 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 2.6479 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
384.05 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 2.648 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
384.1 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 3.807 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
552.2 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 4.9018 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
710.95 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
 4.9019 MPa
@Treatment Temp. 100 °C,
Time 252000 sec
710.96 psi
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 592 %592 %
 287.7 %
@Treatment Temp. 100 °C,
Time 252000 sec
287.7 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 287.7 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
287.7 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel B
 381.84 %
@Treatment Temp. 100 °C,
Time 252000 sec
381.84 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #3
 513.3 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
513.3 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel A
 516.8 %
@Treatment Temp. 100 °C,
Time 252000 sec
516.8 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Heat Aged
 529.25 %
@Treatment Temp. 100 °C,
Time 252000 sec
529.25 %
@Treatment Temp. 212 °F,
Time 70.0 hour
ASTM Oil #1
100% Modulus 1.14 MPa165 psi
Tear Strength 11.9 kN/m68.0 pliDie B
Compression Set  19.2 %
@Treatment Temp. 100 °C,
Time 79200 sec
19.2 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Solid
 24.9 %
@Treatment Temp. 100 °C,
Time 79200 sec
24.9 %
@Treatment Temp. 212 °F,
Time 22.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.6 °C-32.0 °F
Shrinkage  -3.40 %
@Treatment Temp. 100 °C,
Time 252000 sec
-3.40 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 -2.00 %
@Treatment Temp. 100 °C,
Time 252000 sec
-2.00 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Weight, Heat Aged
 3.4 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
3.4 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel A
 11.5 %
@Treatment Temp. 100 °C,
Time 252000 sec
11.5 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 13.3 %
@Treatment Temp. 100 °C,
Time 252000 sec
13.3 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 40.2 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
40.2 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL008 / 318218

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.