MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Spartech EP5220 Calcium Carbonate Filled Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Calcium Carbonate (CaCO3) Filler

Material Notes: Provides the highest level of stiffness and heat resistance of filled olefins. Calcium Carbonate filled grades offer an excellent balance of stiffness and impact resistance. Typical applications include extrusion/thermoformed food containers, and profile extruded and blown molded structural parts.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc
@Temperature 22.8 °C
1.05 g/cc
@Temperature 73.0 °F
ASTM D792
Filler Content 20 %20 %
Linear Mold Shrinkage 0.015 cm/cm0.015 in/in0.125inch wall
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.3 MPa4400 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Flexural Modulus 1.59 GPa230 ksisecant; ASTM D790
 2.00 GPa290 ksitangent; ASTM D790
Izod Impact, Notched 0.641 J/cm
@Temperature 22.8 °C
1.20 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact  2.71 J
@Temperature -5.56 °C
2.00 ft-lb
@Temperature 22.0 °F
ASTM D5420
 19.0 J
@Temperature 22.8 °C
14.0 ft-lb
@Temperature 73.0 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C130 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 75 %75 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer
Spartech PP7220 Calcium Carbonate Filled High Impact Copolymer
Spartech PP5240 Calcium Carbonate Filled Homopolymer

PSPAR127 / 78749

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.