MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Spartech PP5240 Calcium Carbonate Filled Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Calcium Carbonate (CaCO3) Filler

Material Notes: Offers improved stiffness versus unfilled materials. They offer substantial improvements in drop weight (Gardner) impact over both unfilled polypropylene and other types of filled polypropylene. Calcium Carbonate also offers advantages in appearance, gloss, and colorability due to its bright white color.

Information provided by Spartech

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.25 g/cc
@Temperature 22.8 °C
1.25 g/cc
@Temperature 73.0 °F
ASTM D792
Filler Content 40 %40 %
Linear Mold Shrinkage 0.010 cm/cm0.010 in/in0.125inch wall
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.1 MPa3500 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Elongation at Yield 5.0 %5.0 %ASTM D638
Flexural Modulus 1.79 GPa260 ksisecant; ASTM D790
 2.34 GPa340 ksitangent; ASTM D790
Izod Impact, Notched 0.374 J/cm
@Temperature 22.8 °C
0.700 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 24.4 J
@Temperature 22.8 °C
18.0 ft-lb
@Temperature 73.0 °F
ASTM D5420
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °C240 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C133 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 50 %50 %60°; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer
Spartech PP7220 Calcium Carbonate Filled High Impact Copolymer
Spartech PP5220 Calcium Carbonate Filled Homopolymer
Spartech EP6240 Filled and Reinforced Copolymer
Spartech EP6220 Filled and Reinforced Copolymer

PSPAR116 / 78738

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.