MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Unfilled

Material Notes: AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.

Applications:

  • Components for automotive and aircraft engines
  • Transmission
  • Farming, off-road and construction equipment
  • Industrial machinery
  • Electric motors, pumps and compressors
  • Business machines such as laser pointers and high speed copy machines
  • Electronic and semiconductor transport media
  • Analytical and medical equipment
  • Conveyors and textile equipment

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/ccASTM D792
Water Absorption 0.34 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.24 %24 hours, 23°C, 60% RH
Linear Mold Shrinkage 0.0083 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 95ASTM D785
Hardness, Rockwell R 129ASTM D785
Tensile Strength at Break 92.2 MPaASTM D638
Tensile Strength, Ultimate 57.9 MPa
@Temperature 150 °C
ASTM D638
Elongation at Break 90 %ASTM D638
 90 %
@Temperature 150 °C
ASTM D638
Flexural Strength 137 MPaASTM D790
 88.3 MPa
@Temperature 150 °C
ASTM D790
Flexural Modulus 2.94 GPaASTM D790
 2.55 GPa
@Temperature 150 °C
ASTM D790
Compressive Strength 780 kg(f)/cm²
@Temperature 150 °C
JIS K7208
 1220 kg(f)/cm²
@Temperature 23.0 °C
JIS K7208
Compressive Modulus 1.57 GPaAt 150°C; JIS K7208
 2.16 GPaAt 23°C; JIS K7208
Shear Strength 78.5 MPa
@Temperature 150 °C
JIS K7214
 81.4 MPa
@Temperature 23.0 °C
JIS K7214
Izod Impact, Notched 9.00 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cmASTM D257
Surface Resistance 1.00e+17 - 1.00e+18 ohmASTM D257
Dielectric Constant 3.1
@Frequency 1e+6 Hz
ASTM D150
 3.2
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.00090
@Frequency 1000 Hz
ASTM D150
 0.0034
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 55.0 µm/m-°C
@Temperature 23.0 °C
MD; ASTM D696
 55.0 µm/m-°C
@Temperature 200 °C
MD; ASTM D696
CTE, linear, Transverse to Flow 55.0 µm/m-°C
@Temperature 23.0 °C
ASTM D696
 55.0 µm/m-°C
@Temperature 200 °C
ASTM D696
Specific Heat Capacity 1.00 J/g-°C
@Temperature 23.0 °C
By DSC
 1.00 J/g-°C
@Temperature 100 °C
By DSC
 1.42 J/g-°C
@Temperature 300 °C
By DSC
Thermal Conductivity 0.000417 cal cm/sec-cm²-°C
Melting Point 388 °C
Maximum Service Temperature, Air 238 °CHeat distortion temperature, load unknown; ASTM D648
Glass Transition Temp, Tg 250 °CBy DSC
Decomposition Temperature 570 °C5% weight reduction temperature, by DTG
Flammability, UL94 V-0
@Thickness 0.400 mm
all color
 5VA
@Thickness 2.00 mm
all color
Oxygen Index 47 %
@Thickness 3.20 mm
ASTM D256
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 420 °CInjection molding, extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Sintimid™ V Unfilled Polyimide (PI)
Mitsui AURUM® PL450C Polyimide
Mitsui AURUM® PL6200 Thermoplastic Polyimide Resin, Non-filled
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined

PMIT036 / 53212

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.