Nicro-45 air hardened, high alloy steel is intended specifically for applications requiring a high degree of abrasion and wear resistance. Unlike normal quenched and tempered material, high-heat cycling with air-cooling alone will not result in loss of hardenability and wear resistance. Used by industries such as mining, forestry, quarrying and construction. Nicro 45 is the cost-effective choice for parts subjected to extremely high levels of wear. Information from Wingate Alloys Inc. |