MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Wingate Alloys Nicro 45 Ultra High Strength Alloy Wear Plate
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Nicro-45 air hardened, high alloy steel is intended specifically for applications requiring a high degree of abrasion and wear resistance.

Unlike normal quenched and tempered material, high-heat cycling with air-cooling alone will not result in loss of hardenability and wear resistance. Used by industries such as mining, forestry, quarrying and construction. Nicro 45 is the cost-effective choice for parts subjected to extremely high levels of wear.

Information from Wingate Alloys Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 420 - 465
Tensile Strength 210000 psi
Tensile Strength, Yield 181000 psi
Elongation at Break 11.5 %2[in]
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.0040 %
Carbon, C 0.25 %
Chromium, Cr 1.6 %
Iron, Fe 92.916 %
Manganese, Mn 1.0 %
Molybdenum, Mo 0.35 %
Nickel, Ni 3.5 %
Phosphorus, P 0.30 %
Silicon, Si 0.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ArcelorMittal Usibor® 1500 Ultra high strength steel, Cold Rolled
AISI 4817 Steel
AISI 4820 Steel, annealed 815°C (1500°F)
AISI 4820 Steel, direct quenched from pot, tempered 150°C (300°F), 0.99 mm case depth
AISI 8115 Low Alloy Steel, Cold Drawn Bar

NWINGA04 / 122068

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.