MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Asahi Kasei ASACLEAN PF Purging Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Asaclean PF is formulated for super-engineering resins at processing temperatures of up to 420°C (790°F). PF Grade is suitable for Hot Runner cleaning. PF can be used as a sealing material during machine shutdowns within the temperature ranges of 280°-370°C (535°-700°F) due to its superior thermal stability.

Information provided by Asaclean.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 280 - 420 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bakelite® PF 31 Phenolic Formaldehyde Resin, UL Listed
Bakelite® PF 7596 Phenolic Molding Compound
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
Bakelite® PF 1110 Phenolic Molding Compound

PACLEAN10 / 176001

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.