MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPV K 156 BLK Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink K-156 is a high performance thermoplastic vulcanizate designed for a variety of automotive applications including exterior parts. This grade has superior low temperature performance and is suitable for injection molding.

Availability: Europe

Features: Chemical Resistant; Good Mold Release; High Hardness; Low Density; Low Specific Gravity; Low Temperature Impact Resistance

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Automotive Specifications: GM QK 003531 Color: Black; PSA Peugeot-Citroen B62 0300 version G Color: Black; RENAULT F.R.M. 4D-50-A08 Color: Black; RENAULT F.R.M. 4D-50-A09 Color: Black; VAG VW501 23 Color: Black; VAG VW-TL 526 22-MD01 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO 1183
Viscosity 198 cP
@Shear Rate 206 1/s,
Temperature 200 °C
Apparent Shear; ISO 11443
Linear Mold Shrinkage 0.0010 - 0.016 in/in
@Thickness 2.00 mm
ISO 294-4
Melt Flow 70 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 38
@Time 5.00 sec
Injection Molded, Change in Air, 168; ISO 868
Tensile Strength at Break 1480 psiAcross Flow; ISO 37
Tensile Stress at Strain 1150 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 570 %Across Flow; ISO 37
Flexural Modulus 38400 psi
@Temperature 22.8 °C
ISO 178
 155000 psi
@Temperature -40.0 °C
ISO 178
Izod Impact, Notched (ISO) NB
@Temperature -35.0 °C
ISO 180/A
Compression Set 74 %
@Temperature 70.0 °C,
Time 79200 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 350 - 420 °F
Middle Barrel Temperature 350 - 420 °F
Front Barrel Temperature 350 - 420 °F
Nozzle Temperature 360 - 430 °F
Melt Temperature 360 - 430 °F
Mold Temperature 50.0 - 150 °F
Drying Temperature 180 °F
Dry Time 3.00 hour
Back Pressure 10.0 - 150 psi
Screw Speed 100 - 200 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1203 / 237694

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.