MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV K 156 BLK Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink K-156 is a high performance thermoplastic vulcanizate designed for a variety of automotive applications including exterior parts. This grade has superior low temperature performance and is suitable for injection molding.

Availability: Europe

Features: Chemical Resistant; Good Mold Release; High Hardness; Low Density; Low Specific Gravity; Low Temperature Impact Resistance

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim

RoHS Compliance: RoHS Compliant

Automotive Specifications: GM QK 003531 Color: Black; PSA Peugeot-Citroen B62 0300 version G Color: Black; RENAULT F.R.M. 4D-50-A08 Color: Black; RENAULT F.R.M. 4D-50-A09 Color: Black; VAG VW501 23 Color: Black; VAG VW-TL 526 22-MD01 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ISO 1183
Viscosity 198 cP
@Shear Rate 206 1/s,
Temperature 200 °C
198 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent Shear; ISO 11443
Linear Mold Shrinkage 0.0010 - 0.016 cm/cm
@Thickness 2.00 mm
0.0010 - 0.016 in/in
@Thickness 0.0787 in
ISO 294-4
Melt Flow 70 g/10 min
@Load 5.00 kg,
Temperature 230 °C
70 g/10 min
@Load 11.0 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 38
@Time 5.00 sec
38
@Time 0.00139 hour
Injection Molded, Change in Air, 168; ISO 868
Tensile Strength at Break 10.2 MPa1480 psiAcross Flow; ISO 37
Tensile Stress at Strain 7.93 MPa
@Strain 100 %
1150 psi
@Strain 100 %
Across Flow; ISO 37
Elongation at Break 570 %570 %Across Flow; ISO 37
Flexural Modulus  0.265 GPa
@Temperature 22.8 °C
38.4 ksi
@Temperature 73.0 °F
ISO 178
 1.07 GPa
@Temperature -40.0 °C
155 ksi
@Temperature -40.0 °F
ISO 178
Izod Impact, Notched (ISO) NB
@Temperature -35.0 °C
NB
@Temperature -31.0 °F
ISO 180/A
Compression Set 74 %
@Temperature 70.0 °C,
Time 79200 sec
74 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 216 °C350 - 420 °F
Middle Barrel Temperature 177 - 216 °C350 - 420 °F
Front Barrel Temperature 177 - 216 °C350 - 420 °F
Nozzle Temperature 182 - 221 °C360 - 430 °F
Melt Temperature 182 - 221 °C360 - 430 °F
Mold Temperature 10.0 - 65.6 °C50.0 - 150 °F
Drying Temperature 82.2 °C180 °F
Dry Time 3.00 hour3.00 hour
Back Pressure 0.0689 - 1.03 MPa10.0 - 150 psi
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1203 / 237694

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.